PubMed-ID: 21479287Seiten: 172-174, Sprache: EnglischØilo, Marit / Tvinnereim, Helene M. / Gjerdet, Nils RoarThe aim of this study was to evaluate the damage tolerance of different zirconia-based materials. Bars of one hard machined and one soft machined dental zirconia and an experimental 95% zirconia 5% alumina ceramic were subjected to 100,000 stress cycles (n = 10), indented to provoke cracks on the tensile stress side (n = 10), and left untreated as controls (n = 10). The experimental material demonstrated a higher relative damage tolerance, with a 40% reduction compared to 68% for the hard machined zirconia and 84% for the soft machined zirconia.