Open AccessPubMed ID (PMID): 25911826Pages 9-20, Language: English, GermanFrankenberger, Roland / Hartmann, Vera E. / Krech, Michael / Krämer, Norbert / Reich, Sven M. / Braun, Andreas / Roggendorf, Matthias J.
Objective: To evaluate the adhesive bonding performance of recently introduced tooth-colored CAD/CAM materials after different pretreatment protocols and using different luting materials.
Materials and methods: The CAD/CAM materials under investigation were e.max CAD (lithium disilicate glass ceramic; Ivoclar Vivadent, Schaan, Liechtenstein), Celtra Duo (zirconia-reinforced lithium disilicate ceramic; Dentsply DeTrey, Konstanz, Germany), Lava Ultimate (resin nano ceramic; 3M ESPE, Neuss, Germany), and Enamic (resin infiltrated ceramic; Vita, Bad Säckingen, Germany). A total of 240 blocks (n = 5) received various pretreatments (no pretreatment, silane, sandblasting, sandblasting + silane, hydrofluoric acid, hydrofluoric acid + silane), and then different classes of adhesive luting composites were applied (adhesive: Prime&Bond XP + SCA + Calibra; Dentsply DeTrey; self adhesive: RelyX Unicem; 3M ESPE). After 24 h water storage and 10,000 thermocycles (5°C/55°C), specimens were cut into beams and microtensile bond strengths were recorded.
Results: Bonding performance of recent CAD/CAM materials was clearly influenced by the pretreatment method (P < 0.05). In general, significantly higher μ-TBS values were recorded for the ceramic materials compared to the hybrid materials (P < 0.05). Among the hybrid materials, Enamic exhibited higher bond strengths than Lava Ultimate (P < 0.05). However, despite the differences found, all materials showed a high level of bonding performance, being sufficient to withstand intraoral chewing forces during mastication.
Conclusion: When pretreated as recommended by the manufacturers, recent tooth-colored CAD/CAM materials show an encouraging bonding performance for adhesive luting.
Keywords: adhesive luting, CAD/CAM, ceramics, enamel, dentin, hybrid materials, resin composite